Dear industry colleagues,
Not infrequently off line e-mail arrives which is often both illuminating and
thought provoking. The following material is from one such message, in this
case, from a contract manufacturer who has some posed some technical and
logistical questions regarding conversion to lead-free that are likely being
faced by most if not all contract assemblers.
I received permission from them to post the following for general comment.
Please consider this a "from the trenches" request from an individual on the
front lines.
Comments, suggestions or ideas relative to the points made should preferably
be posted on the forum, however, if you prefer, I can take your comments off
line and forward them to the sender.
Thanks in advance for sharing your thoughts/comments.
Kind regards to all,
Joe
"1. As a contract manufacturer, we have many customers with many designs,
and many different component part numbers. It is not clear who will be
responsible for identifying which components can handle the longer hotter
reflow cycles or wave process. I am sure the burden will be shared as some
customers will request the change and others may accept the change.
2. I am not as concerned about the bare board materials as I am about the
individual components. For each component, the reliability and functionality
needs to be reviewed -- especially components that are Moisture Sensitive
Devices as those have been qualified under the 63/37 reflow melting
temperatures.
3. Identifying, Categorizing, and Separating inventories for customers with
lead-free vs. not lead free is going to be a logistical nightmare. Keep in
mind, if there is no legislation in the US and some of our customers are
happy with the current alloy they will have no reason to change and CM's will
need to keep inventories straight.
4. Many companies have a difficult time keeping No-Clean and Water Soluble
chemistries from being mixed -- Imagine if we need to keep Lead-Free No-Clean
and Lead-Free Water Soluble chemistries away from the Leaded No-Clean and
Water Solubles?
5. Equipment -- A second Wave machine will be needed, center support rails
on the reflow ovens will be needed to support the PCB's that sag under higher
heat, increased machine maintenance will be needed, and imagine how the cost
of electricity will go up along with the cost of increased AC! What about
Nitrogen -- We'll probably need to add that with the board finishes and
higher temps. How will X-ray work without Lead? How will Vision systems
work as the reflectivity of the solder joints change?
This just touches the tip of the iceberg.
I suppose what confuses me the most is the cost. Is the cost of this all
justified? Has anyone done a cost/benefit analysis?
I am also confused when I hear that Silver is one of the elements used in one
of the more promising alloys. Is the risk and high toxicity level associated
with mining and refining silver far less than the toxicity of the lead that
ends back up in the ground (where it started in the first place?)
And what about the guy who dumps his battery on the side of the road so he
doesn't have to pay $5 to get rid of it properly?
Well, I suppose that's enough for one night. It was kind of fun to be on
the soap box for a few minutes and relieve some of the stress about what
might become inevitable."
---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|