The best type of "lock washer" I have ever run across is a Schnorr
washer, they are serrated Belleville washers, we have used them in our
military systems, and they held when nothing else would.
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Stadem, Richard D.
> Sent: Thursday, October 12, 2006 3:02 PM
> To: [log in to unmask]
> Subject: Re: [TN] Compression Limit on FR4?
>
> Hi, Jack
> I can tell you that typically the torque setting used for hardware on
> pwb assemblies is between 1 to 6 in/lbs. More than that tends to
deform
> the fiberglass over time. Of course, it all depends on the type of
board
> material, layer count, etc.
> It also depends on the application.
> Realize that a lot of relaxation occurs during any type of thermal
> excursion, and the hardware will loosen up. It is always a good idea
to
> use a Bellville washer in conjunction with a serrated or star washer
to
> continue to hold the torque. It is also a good idea to use Glyptol or
> some other threadlocker.
>
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Jack Olson
> Sent: Thursday, October 12, 2006 1:54 PM
> To: [log in to unmask]
> Subject: [TN] Compression Limit on FR4?
>
> Does anyone know of any guidelines or recommendations that suggest a
> maximum limit on compressing board material?
>
> Can any damage occur by over-torque'n screws, for example?
>
> I've never heard anyone discuss that...
>
> Jack
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
> unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt
or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
> archives of previous posts at: http://listserv.ipc.org/archives Please
> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for
> additional information, or contact Keach Sasamori at [log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
http://listserv.ipc.org/archives
> Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at
[log in to unmask] or
> 847-615-7100 ext.2815
> -----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|