TECHNET Archives

November 2016

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
GRIVON Arnaud <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, GRIVON Arnaud <[log in to unmask]>
Date:
Wed, 2 Nov 2016 15:56:42 +0100
Content-Type:
text/plain
Parts/Attachments:
text/plain (13 lines)
Hello,

Does anyone has return of experience or feedback regarding the use of solderable enamelled copper wires for jumpers or wire repairs on Class 3 PCBAs?
Any potential limitations or restrictions of use?
The one that is considered is a 36AWG/0.19mm wire.

This seems not to be clearly addressed in the IPC 7711/7721.
I only found the following mention (IPC-7721B §6.1, Jumper Wires) : Recommended wire is solid insulated plated copper wire, tin lead plated, 22 to 32 AWG with Kynar, Milene, Kapton, Teflon or equivalent insulation.

Thanks in advance.