We stencil print with 8 mil thick stainless steel stencils... 0603 = 20 mil
dia and 0805 = 28 mil dia
bill...
At 11:54 AM 03/13/2002 -0500, you wrote:
>We dispense glue using a positive displacement pump.
>Dot diameter for 0603's is nominally 20 mils.
>Dot diameter for 0805's is nominally 28 mils.
>Dick Krug
>Sypris Electronics
>
>-----Original Message-----
>From: Vinit Verma [mailto:[log in to unmask]]
>Sent: Wednesday, March 13, 2002 7:19 AM
>To: [log in to unmask]
>Subject: [TN] Glue Dot Size
>
>
>Hi All,
>
>Has anyone ever worked with the Pump Printing Stencil for printing glue on
>pre-inserted PCBs?? This stencil is developed by DEK but I'm not too sure of
>how it works? Any experiences?
>
>Also would be too kind if somebody could tell me the glue size requirement
>for 0603 and 0805 components?
>
>Thanks in advance
>
>Regards
>Vinit Verma
>
>----------------------------------------------------------------------------
>-----
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
>Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
>E-mail Archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>----------------------------------------------------------------------------
>-----
>
>---------------------------------------------------------------------------------
>Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
>To unsubscribe, send a message to [log in to unmask] with following text in
>the BODY (NOT the subject field): SIGNOFF Technet
>To temporarily halt delivery of Technet send e-mail to [log in to unmask]:
>SET Technet NOMAIL
>To receive ONE mailing per day of all the posts: send e-mail to
>[log in to unmask]: SET Technet Digest
>Search previous postings at: www.ipc.org > On-Line Resources & Databases >
>E-mail Archives
>Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
>information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
>ext.5315
>---------------------------------------------------------------------------------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|