Mime-Version: |
1.0 |
Content-Type: |
text/plain; charset="ISO-8859-1"; Name="Message Body" |
Old-Return-Path: |
|
Date: |
16 Jul 1996 16:28:58 -0400 |
Precedence: |
list |
Resent-From: |
|
Resent-Sender: |
|
From [log in to unmask] Tue Jul 16 17: |
40:43 1996 |
Status: |
O |
X-Mailing-List: |
|
TO: |
|
Return-Path: |
<TechNet-request> |
X-Status: |
|
X-Loop: |
|
Resent-Message-ID: |
<"INgrl.0.mQM.i50xn"@ipc> |
Subject: |
|
From: |
|
Received: |
by ipc.org (Smail3.1.28.1 #2)
id m0ugH89-00009uC; Tue, 16 Jul 96 15:54 CDT |
Content-Transfer-Encoding: |
quoted-printable |
X-Mailer: |
Mail*Link SMTP-QM 3.0.1 |
Message-Id: |
|
Parts/Attachments: |
|
|
Subject: Time: 4:28 PM
OFFICE MEMO ASSY: TSOP Underfilling? Date: 7/16/96
We have been using TSOP (Thin Small Outline Packages), both type I and II configurations, reliably for several years on relatively thick boards (63-110 mils thick) without any underfill. I've heard of problems with the solder joints of these devices when they're used on thin boards - we have a board that looks like it will be about 31 mils thick. Some people have described the need for an epoxy underfill to dampen the stresses at the solder joints. Can anybody comment on this?
Thanks for any assistance!
Greg Bartlett
Mercury Computer Systems
Chelmsford, MA
[log in to unmask]
***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to: *
* [log in to unmask] with <subject: unsubscribe> and no text. *
***************************************************************************
|
|
|