Hi Dave!
Got your "Barney Boards" presentation and it's posted here:
http://stevezeva.homestead.com/Case_studies_Barney_boards.ppt
Steve
On Mon, Jul 21, 2014 at 11:00 AM, David Hillman <
[log in to unmask]> wrote:
> Hi Steve - here is Doug's and my picture of purple solder joints out of
> one of our ppts you can post:
>
> Dave
>
>
> On Mon, Jul 21, 2014 at 10:43 AM, Steve Gregory <[log in to unmask]>
> wrote:
>
>> Hi Dick!
>>
>> I've seen that too after cleaning with some really good DI water. I had
>> solder joints that turned purple on me one time, but they weren't wave
>> soldered, and it was on a ENIG board and I was using a water soluble SAC
>> 305 paste. Here are some pictures of what I was experiencing:
>>
>> http://stevezeva.homestead.com/Trippy_Solder.jpg
>>
>> http://stevezeva.homestead.com/Trippy_Solder_Close.jpg
>>
>> I could "Buff" the purple color away with a stiff bristled solder joint
>> just as long as I polished the surface well. Here are some before and
>> after
>> pictures of that:
>>
>> http://stevezeva.homestead.com/Before_Buffing.jpg
>>
>> http://stevezeva.homestead.com/After_Buffing.jpg
>>
>> It wasn't a residue, because I measured the cleanliness with an omegameter
>> and it was negligible, and the solder appeared the same.
>>
>> Then a fellow Technetter; George M. Wenger of Failure Signature &
>> Characterization Lab graciously offered to analyze this for me and here's
>> his report:
>>
>> http://stevezeva.homestead.com/FSC-5178.ppt
>>
>> Steve
>>
>>
>> On Mon, Jul 21, 2014 at 8:29 AM, Richard Krug <[log in to unmask]> wrote:
>>
>> > We have recently discovered some CCA's with a distinctive, transparent
>> > blue color on the solder joints. Viewed perpendicular to the solder
>> joint
>> > surface, surface looks normal. The solder surface appears blue when
>> viewed
>> > at an angle. I see no residues at up to 30x magnification. Boards were
>> > wave soldered using Sn63Pb37 solder with ORH1 flux, then in-line water
>> > washed with a low concentration of a saponifier as one of our common
>> > assembly processes.
>> >
>> > Any ideas of what the condition is or what caused it?
>> >
>> > Dick Krug, CSSBB, CSMTPE
>> > Lead Process Engineer
>> > Sparton Brooksville, LLC
>> > 30167 Power Line Road
>> > Brooksville, FL 34602-8299
>> > p (352) 540-4012 (Internal Ext. 2012)
>> > [log in to unmask]
>> >
>> > ______________________________________________________________________
>> > This email has been scanned by the Symantec Email Security.cloud
>> service.
>> > For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> > ______________________________________________________________________
>> >
>>
>> --
>>
>>
>> This email and any attachments are only for use by the intended
>> recipient(s) and may contain legally privileged, confidential, proprietary
>> or otherwise private information. Any unauthorized use, reproduction,
>> dissemination, distribution or other disclosure of the contents of this
>> e-mail or its attachments is strictly prohibited. If you have received
>> this
>> email in error, please notify the sender immediately and delete the
>> original.
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud service.
>> For more information please contact helpdesk at x2960 or [log in to unmask]
>> ______________________________________________________________________
>>
>
>
--
This email and any attachments are only for use by the intended
recipient(s) and may contain legally privileged, confidential, proprietary
or otherwise private information. Any unauthorized use, reproduction,
dissemination, distribution or other disclosure of the contents of this
e-mail or its attachments is strictly prohibited. If you have received this
email in error, please notify the sender immediately and delete the
original.
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|