TECHNET Archives

March 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 1 Mar 2010 23:46:39 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Joyce Koo <[log in to unmask]>
Subject:
From:
Joyce Koo <[log in to unmask]>
Content-Transfer-Encoding:
base64
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (1 lines)
Sorry for the confusion: the 1st generation BGA got lead rich ball (Pb more tha 85%).  You attach use eutectic solder to the PCB.  The high Pb ball never completely melted.  The standoff of the BGA is ensured due to the ball high temp materials used by design.  Similar to the C4 joints made by 95% Pb. 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: vladimir Igoshev <[log in to unmask]>
To: TechNet E-Mail Forum <[log in to unmask]>; Joyce Koo
Sent: Mon Mar 01 23:30:48 2010
Subject: Re: [TN] BTC rework, Square SJs

Joyce,

You sound confusing. What do you mean by saying: "... Pb-rich and eutectic solder" in one sentence?

Regards,

Vladimir
Vladimir

SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca

-----Original Message-----
From: Joyce Koo <[log in to unmask]>
Date:         Mon, 1 Mar 2010 23:09:45 
To: <[log in to unmask]>
Subject: Re: [TN] BTC rework, Square SJs

Werner,
Thx for the reply.  However, the old Pb rich ball solder to the board using eutectic can be ensure the proper stand off achieved.  At current lead free, there is a little attention being paid to achieve the proper standoffs.  As for the good workmanship and process, regardless the size and cte mismatch, should ipc establish a proper guideline, if not spec for establish % collapse of ball standoff requirements?  Rather than depends upon individual case of cte, parts?  I have seen some squarches bga joints almost look like LGAs.  Sure it is not "good".  Can't wait for rel data to establish each of them.  Can so guru come out a number that universally acceptable?  At least meet the "intend of the design" in term of reliability.  Any takers?  
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Mar 01 19:09:37 2010
Subject: Re: [TN] BTC rework, Square SJs


 Joyce,
That depends on the reliability you want to achieve, the package size, the delta-CTE and the cyclic delta-T.

Werner
Upcoming workshops:
May 21, IPC Int. Conference on Reliability and Quality of Lead-Free Electronics, Frankfurt, Germany,
      “Reliability Issues and Solution Options for Pb-Free Soldered Electronic Products”
May 26, FED Seminar, Stuttgart, Germany,
     “Bleifreie Lötprozesse—Frühausfälle, Qualität, Zuverlässigkeit”
June 8, SMT/HYBRID/PACKAGING 2010, Nürnberg, Germany,
     “Reliability Issues with Lead-Free Soldering”



 


 

 

-----Original Message-----
From: Joyce Koo <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Mar 1, 2010 6:09 pm
Subject: Re: [TN] BTC rework, Square SJs


Warner, 
What is the max collapse allowable of ball from its height? 
--------------------------
Sent using BlackBerry


----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Mar 01 13:56:14 2010
Subject: Re: [TN] BTC rework, Square SJs


 Hi Chris,
The problem with this SJ is the low solder joint height 9=reduced reliability) 
and the stress concentration geometry from SMD.
Werner

 


 

 

-----Original Message-----
From: Chris Mahanna <[log in to unmask]>
To: Werner Engelmaier <[log in to unmask]>; [log in to unmask] <[log in to unmask]>
Sent: Mon, Mar 1, 2010 1:08 pm
Subject: RE: [TN] BTC rework, Square SJs



In cross section, the vertical sides of the joint are straight. I assume it has 
more/less retained the shape of the [trapezoidal?] stencil.
Chris
 

From: Werner Engelmaier[mailto:[log in to unmask]] 
Sent: Monday, March 01, 2010 12:52 PM
To: [log in to unmask]; Chris Mahanna
Subject: Re: [TN] BTC rework, Square SJs

 

Chris,
What do you mean by "squarejoints?"
Werner

 

 

-----Original Message-----
From: Chris Mahanna <[log in to unmask]>
To: [log in to unmask]
Sent: Mon, Mar 1, 2010 12:15 pm
Subject: [TN] BTC rework, Square SJs

Are square joints simply due to the small mass of the components, or is it 




possibly an indicator of insufficient heat?  We have no indication that any of 




the paste didn't flow.  Wetting looks good.  All evidence is from microsection.









Thanks,




Chris









______________________________________________________________________




This email has been scanned by the MessageLabs Email Security System.




For more information please contact helpdesk at x2960 or [log in to unmask] 




______________________________________________________________________









---------------------------------------------------




Technet Mail List provided as a service by IPC using LISTSERV 15.0




To unsubscribe, send a message to [log in to unmask] with following text in




the BODY (NOT the subject field): SIGNOFF Technet




To temporarily halt or (re-start) delivery of Technet send e-mail to 




[log in to unmask]: SET Technet NOMAIL or (MAIL)




To receive ONE mailing per day of all the posts: send e-mail to 




[log in to unmask]: SET Technet Digest




Search the archives of previous posts at: http://listserv.ipc.org/archives




Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 




additional information, or contact Keach Sasamori at [log in to unmask] or 




847-615-7100 ext.2815




-----------------------------------------------------











 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, please 
immediately reply to the sender and delete this information from your system. 
Use, dissemination, distribution, or reproduction of this transmission by 
unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for 
additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

 

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________


---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2