Paul Wilson <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Eltek Ltd. - Process Engineering" <[log in to unmask]>
Parts/Attachments:
text/plain (58 lines)
At 10:50 02/04/98 -0500, you wrote:
>Edward Szpruch,
>Eltek Ltd - Israel
>
>Actually, I would like to hear about the results of your decision making
process.  Denny Fritz of Macdermid, Waterbury, Connecticut, claims to have a
system capable of 2/2 with new transport and alkaline etchant with 90+%
yields:  sounds a little too good to be true.  Maybe there's a customer who
can confirm?
>
>Paul G. Wilson
>Plant Chemist
>Circuit Center, Inc.

Paul !
I met Danny Fritz of Macdermid in the past . I don`t know , what kind of
equipment they have now . Macdermid become to be supplier of the equipment
following their joint venture with Hollmuller on US market . Couple years
ago Hollmuller was recognised as first class manufacturer of equipment ,
equal to Schmid .
Later on , Macdermid took the part of Hollmuller and now they are competing
, even on europiean market .
Schmid is now the lonely leader , but their prices are very high !!
By the way , to make 2/2 conductors , etching is just the end of the chain .
What about image transfer , plating ( for tend and etch or pattern plating +
plating resist stripping ! )
 I had such discussion with my boss regarding warranty conditions for such
equipment : I told , that we are buying pile of plastics , shafts and
electricity wires . I don`t know , what kind of " net " performance tests
might be imposed on the manufactorer of the machinery ...
For outerlayers nothing special is required from transportation system ,
because outerlayers are self-supported . Rest of the stuff is mixed
chemistry and machinery :
1 ) proper and controlable spray profile , especially top manifolds .
2 ) properly chosen chemistry ( rather low and fixed pH , stable chlorides ,
adequate aeration etc ) .
3 ) Untill now no one of Pill`s users responded ... Their machinery looks
very nice and have reasonable price .
I hope You got some idea about my decision making . By the way , we are
manufacturing from time to time 2 mills wide conductors or even less  , but
not on purpose ( on the artwork they were 5 )
Edward

>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2