TECHNET Archives

April 2016

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Yuan-chia Joyce Koo <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Yuan-chia Joyce Koo <[log in to unmask]>
Date:
Mon, 11 Apr 2016 20:15:43 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (20 lines)
Ta cap have self healing (if done properly) capability, function  
within spec and design within the margin, should be OK, unless you  
got from non-proven  source  (parts... there are Ta caps that would  
blow, just a little over the spec....).
my 1.5 cents.
       jk
On Apr 11, 2016, at 7:45 PM, Julie Silk wrote:

> Are you sure the blown tantalum capacitor was a result of the  
> failure and not the cause of it?  That is, if the cap blew, would  
> this cause the overheating that spewed molten solder out of the  
> via?  Ta caps can fail with the right (wrong) circumstances, even  
> if loaded correctly.


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2