It's interesting and logic in the explanation below. But more
important is how to prevent it. Any suggestion?
Regards,
KenF
______________________________ Reply Separator _________________________________
Subject: Re: [TN] Electromigration of Tin Lead?
Author: "TechNet E-Mail Forum." <[log in to unmask]> [log in to unmask] at
Internet
Date: 5/26/99 2:26 PM
Hi Phil,
The "feathery migration tracks" you are describing are most likely dendritic
growth, sometimes called 'Conductive Anodic Filaments (CAF)'. Dendritic
growth starts as the migration of metal, and other salts, along paths created
by structural imperfections. This migration requires moisture, water in most
cases, but the presence of an electrical potential is not necessary. When
electrical potential is applied, the migration is more rapid and organizes
itself into CAF. CAF leads to a reduction in insulation resistance, and
depending on the currents present can create localized shorts and burn-out.
Werner Engelmaier
Engelmaier Associates, L.C.
Electronic Packaging, Interconnection and Reliability Consulting
7 Jasmine Run
Ormond Beach, FL 32174 USA
Phone: 904-437-8747, Fax: 904-437-8737
E-mail: [log in to unmask], Website: www.engelmaier.com
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
textin the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|