Pat,
MIL-I-46058 is the mil spec on conformal coatings. It was declared
inactive for new designs in 1995. The only reason it is still around is
the QPL list for it. Way outdated and it only gives a minimum set of
criteria to reach and is not really a performance spec.
Doug Pauls
From: "Goodyear, Patrick" <[log in to unmask]>
To: "'TechNet E-Mail Forum'" <[log in to unmask]>,
"[log in to unmask]" <[log in to unmask]>
Date: 03/07/2013 10:39 PM
Subject: RE: [TN] Conformal Coating and J1 / 610
Doug,
What do the Mil Specs say concerning conformal coatings? It has been 31
years since I played in that field, but I remember they use to have very
specific requirements. Just another reference source.
pat
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Thursday, March 07, 2013 8:06 AM
To: [log in to unmask]
Subject: [TN] Conformal Coating and J1 / 610
Greetings Citizens of the Galactic Empire. You have all been annexed and
the Republic is dissolved. You are now all my minions.
If you do not have an open can of toluene on YOUR desktop, you miss out on
some wonderful hallucinations.
At the recent IPC Apex meetings, as the Chairman of the Cleaning and
Coating groups, I was asked to tackle the conformal coat provisions in
IPC-J-STD-001 and IPC-A-610. I agreed (Proof positive I am an idiot).
Leave it alone Dewey. The coating groups have known for a long time that
these documents need attention, and the time is right at both of those
documents move towards Revision F.
To assist the small working group that is/will be working on this over the
next 6 months, I plan on making use of this forum to gather information. I
have always been impressed by the summary wisdom of Technet.
So, first question:
1. With J-STD-001 and/or IPC-A-610, what areas are NOT presently
addressed, but need to be?
The Death Star will be dispatched to those areas not participating.......
Doug Pauls
Chairman, IPC Cleaning and Coating Committees Galactic Emperor
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
PG&E is committed to protecting our customers' privacy.
To learn more, please visit
http://www.pge.com/about/company/privacy/customer/
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|