Wire bonders should always be isolated from noticeable vibration. For manual
wire bonders you can use table top anti-vibration plates. Its been a lot of
years since I had to use them and can't remember sources. I've never used,
nor would I attempt to use, automatic wire bonders on a raised floor.
Good Luck,
Bruce Misner
> ----------
> From: Oscar M.Alinabon,Jr.[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;[log in to unmask]
> Sent: Monday, May 28, 2001 7:50 PM
> To: [log in to unmask]
> Subject: [TN] Vibration on Raised Floor
>
> Hello Fellow Technets all Around the World !
>
> Can anyone share their experience on raised floor vibration? We have a 2
> ft raised floor assembly and we are experiencing vibrations on our
> equipment particularly wirebonders. We have several options in mind, but I
> would like to get first hand info on
> your experiences. How do you contain such vibrations?
>
> Thanks and best regards
>
>
> Oscar M.Aliņabon,Jr.
> Tel Nos. (632)8445139 ext.288
> Process Engineering Group
> (6349)5430001 to 25 ext 288
> RF Personal Communications &Consumers
> Fax Nos. ( 6349) 5439368
> Philips Semiconductors Philippines Inc.
> email: [log in to unmask]
> Philips Avenue, Light Industry and Science Park 1
> Bo.Diezmo Cabuyao Laguna Philippines 4025
>
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send the following message: SET
> Technet NOMAIL
> Search previous postings at: www.ipc.org > On-Line Resources & Databases >
> E-mail Archives
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
> additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|