Ceramic substrates are typically not produced by a PCB fabrication house but
rather by a thick film house. For solder assembly the metallization is
usually PdAg and it is best soldered with Sn62 instead of Sn63.
Bruce Misner
> ----------
> From: bonilla_d[SMTP:[log in to unmask]]
> Reply To: TechNet E-Mail Forum.;bonilla_d
> Sent: Monday, July 22, 2002 2:39 PM
> To: [log in to unmask]
> Subject: [TN] FW: PCB with Ceramic as substrate
>
> -----Original Message-----
> From: bonilla_d [mailto:[log in to unmask]]
> Sent: Monday, July 22, 2002 2:18 PM
> To: [log in to unmask]
> Subject: PCB with Ceramic as substrate
>
>
> Hi
>
> May somebody give me some a feedback from PCB fabrication house or Process
> Guidelines to deal with this kind of substrate?
>
> Regards
>
> David J Bonilla
> Manufacturing Technology Services
> Phone:787-746-1823 ext 241
> Fax: 787-746-3338
>
> --------------------------------------------------------------------------
> -------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
> ext.5315
> --------------------------------------------------------------------------
> -------
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|