We evaluated some Laser and Selective soldering systems 3 years ago and we
went with Selective soldering systems for the following reasons.
Much larger thru-put capacity. One joint at a time on Laser vs.
multiples on a Selective.
Higher consumable cost on a Laser, Diode pump, Laser rod.
Focus and pin-point accuracy of the Laser was very important, any
shifting, sagging, or bowing of the pwa results in poor/no soldering or
burn boards.
The negative of the Selective soldering is that you need Nitrogen to
promote wetting and reduce dross.
Regards;
Francis Sun
"Ray, Carl (GE
Indust, GE
Fanuc)" To
<carl.ray@GEFANUC [log in to unmask]
.COM> cc
Sent by: TechNet
<[log in to unmask]> Subject
[TN] Laser Soldering vs Selective
Soldering
12/06/2007 08:56
AM
Please respond to
TechNet E-Mail
Forum
<[log in to unmask]>
; Please respond
to
"Ray, Carl (GE
Indust, GE
Fanuc)"
<carl.ray@GEFANUC
.COM>
Hi All,
How many of you "out there" have any experience with laser soldering
machines verse selective soldering machines? Currently we have several
types of selective soldering equipment but due to our designs we are having
significant issues with adjacent components.
I have seen some equipment but do not have experience with the venders or
process.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|