Hi,

My Opinion:

   Unless there was a cost and technical justification for allowing the cap
to remain it is a reject.

Bob K


-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Genny Gibbard
Sent: Friday, February 11, 2011 12:37 PM
To: [log in to unmask]
Subject: [TN] FW: What would you do?

Please see the link below.
Cap under BGA.  
Inquiring minds question: If the board tested out OK, would you ever
consider just leaving this here? The part is a ceramic cap.


________________________________

From: Steve Gregory [mailto:[log in to unmask]]
Sent: February 11, 2011 10:37 AM
To: Genny
 Subject: RE: What would you do?



Hi Genny,

 

I have your picture posted:

 

http://stevezeva.homestead.com/part_under_BGA.jpg

 

It depends. First thing I would want to know, what is this? Is it metal?
If it is, it would be a violation of electrical spacing and I wouldn't leave
it there.

 

Does the ball have any function? Some balls have no function.

What is this board for? A critical application? If it is then no.

How scarce is the BGA?

 

There's a lot of "it depends" that would have to be answered before I would
consider it.

 

My first reaction is that I wouldn't leave it there. But there may be some
circumstances that I might consider it.

 

Steve

 

From: Genny   

 Sent: Friday, February 11, 2011 10:32 AM
To: Steve Gregory
Subject: What would you do?

 

<<part under BGA.jpg>> 

Genny 


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/ContentPage.aspx?Pageid=E-mail-Forums for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2