Hello, I have read several comments regarding "Gold Migration into Tin Lead" 
and have found them both interesting and informative.

I have a similar question:

Does anyone know the results or consequences of Tin/Lead ending up on Gold 
Fingers (as a result of a process problem) which will be inserted into a 
Gold Socket.

All responses would be appreciated and welcomed.

Thankyou

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2