This could be poor drilled hole wall quality that makes plating the
hole wall hole uniformly a challenge. Severe drilled hole roughness
can result in plating folds with areas of thin copper plating. These
areas can pass electrical tests but after thermal exposures they can
break and cause an open via.

Another possiblity is debris left in the hole after drilling can prevent
proper plating of the hole.

X-sections of the open vias should clearly identify the problem.

-- Thanks,
Eddie Rocha
(408) 978-8992 x 282

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2