TECHNET Archives

November 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
Earl Moon <[log in to unmask]>
Date:
Sat, 10 Nov 2001 12:49:02 -0600
X-To:
Werner Engelmaier <[log in to unmask]>
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>
Parts/Attachments:
text/plain (43 lines)
Well said Werner,

However, I am more concerned about surviing operational performance than
simple assembly processes if I am a user of that product.

I?ve never disagreed with the fact we must survive assembly. The old 55110,
and the new one?s, specified that test coupon B, derived from specified
quality conformance test circuitry must be subjected to an extensive
preconditioning period prior to being subjected to a solder ?float? of 550
F. for 10 seconds to ensure the most extreme soldering conditions, during
assembly, would ensure acceptable product. Also, thermal shock conditions
were to be imposed as ?55 C to 125 C in an elevator ride between low and
high temperature chambers simulating PERFORMANCE conditions. Therefore, if
the tests yielded acceptable results, no delamination, in the laminate
evaluation zone, or hole cracking, in the thermal evaluation zone, in
accordance with all that specification?s requirements, it would pass all
assembly processes. In other words, both assembly and performance conditions
would be satisfied and product would be acceptable.

 All this meant if I?m a pilot sitting in my F-16 at 40,000 feet and
counting on going from ground level to that altitude, I certainly would feel
a bit more comfortable if my flight control system assembly was capable of
surviving the thermal transition both as stress and shock. To say the
assembly process is more important and it correlates directly to Tg, is
inadequate. Simply, it is but the first step and if failures exist at the
assembly level, they certainly will during performance ? at altitude as but
one example. AS LONG AS IT WORKS WELL having survived some nearly bad
fabrication/plating processes, I don't care the Tg. After all, we've
successfully used unmodified epoxy resin systems for years even though they
keep getting better.

MoonMan

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2