Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Wed, 18 Sep 2002 05:09:40 -0400 |
Content-Type: | multipart/mixed |
Parts/Attachments: |
|
|
Steve,
I would consider the use of 150-250 uinches of 4-6 wt% NiP under your gold
for bonding.
Steven Creswick - Gentex. Corp
-----Original Message-----
From: Steve kelly [mailto:[log in to unmask]]
Sent: Tuesday, September 17, 2002 4:30 PM
To: [log in to unmask]
Subject: [TN] gold wire bonding
Gold wire bonding - we normally plate electroplated soft gold over
electroplated nickel. Will electroplated soft gold plated on top of
electroless nickel work as well. Thanks. Steve Kelly
PFC Flexible Circuits Limited
----------------------------------------------------------------------------
----- Technet Mail List provided as a free service by IPC using LISTSERV
1.8e To unsubscribe, send a message to [log in to unmask] with following text
in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/html/forum.htm for additional information, or
contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|