TECHNET Archives

January 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="us-ascii"
Old-Return-Path:
Date:
Wed, 22 Jan 1997 09:00:30 -0500
From [log in to unmask] Thu Jan 23 13:
42:25 1997
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/9468
X-Sender:
TO:
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"Wi6Ar3.0.oBM.lhXvo"@ipc>
Subject:
From:
[log in to unmask] (Jack Crawford)
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0vn33Y-0000UDC; Wed, 22 Jan 97 07:49 CST
Message-Id:
<v01540b01af0b85ba3c9a@[204.180.62.40]>
Parts/Attachments:
text/plain (34 lines)
Periodically there are requests for information about assessing and
monitoring solder paste in the manufacturing environment to minimize defect
potential.  Marquette University and the EMPF are presenting a seminar in
Anaheim during NEPCON (Solder Paste Process Control Using AC Electricial
Techniques) to share the results of several years of research with data
collected from several beta test sites.

Contact Dr. Martin Seitz (414) 288-5659 or the EMPF HelpLine directly
(separate from this forum) for more information.

***ALL NEW EMPF PHONE NUMBERS***

Jack Crawford, HelpLine Coordinator
Electronics Mfg. Productivity Facility
****NEW--317.655.3688
****FAX  317-655-3699
714 N Senate Ave, Suite 100
Indianapolis IN  46202-3112
VISIT OUR HOME PAGE AT: http://www.empf.org
[log in to unmask]


***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2