No, but,...
From what I see on their sales flyer (~TDS), performance may be similar to the Dowanol glycol ether line of products.
Likely to depends which one you choose. C7-8 may behave dramatically different than the C13-14 (likely will be the most aggressive).
I would take special note of effect on labels and markings.
Rich Kraszewski
* * * * * * * * CONFIDENTIALITY NOTICE * * * * * * * *
This e-mail and any attachments are confidential from Plexus Corp. and may contain information which is privileged, confidential, and/or protected by non-disclosure agreements. They are intended solely for the use of the named addressee(s). . Any unauthorized use or disclosure may be unlawful. If you are not a named addressee, you must not use, disclose, retain or reproduce all or any part of the information contained in this e-mail or any attachments If you have received this transmission in error, please destroy it and notify us immediately by return e-mail or by calling + 1 888 208 9005.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Douglas Pauls
Sent: Friday, February 8, 2019 1:24 PM
To: [log in to unmask]
Subject: [TN] ISOPAR
[EXTERNAL] This email was sent from outside of Plexus. Use caution when opening attachments or links from unknown senders.
.
Time for a screwy question. Has anyone ever used the fluid ISOPAR to strip acrylic conformal coating? If so, does it work?
*Douglas Pauls *| Principal Materials and Process Engr | Advanced Operations Engineering
*COLLINS AEROSPACE*
400 Collins Road NE, MS 108-101, Cedar Rapids, IA 52498 USA
*Tel:* +1 319 295 2109 | *Mobile: *+1 319 431 3773