TECHNET Archives

September 2008

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Inge <[log in to unmask]>
Date:
Wed, 24 Sep 2008 11:26:52 -0700
Content-Type:
text/plain
Parts/Attachments:
text/plain (167 lines)
Wayne,

For a second or two, that idea flashed by here too, but I thought of all 
specials and tools and things that has to be made to fix it. We resistance 
solder thin lids to small Kovar packages, have a SSEC machine for that, big 
as a house. But it does not have that current capacity. A car 
battery...hmm..not bad idea. Or many in parallel. If one got enough current, 
then time is the other parameter.  I can easily machine heavy copper 
electrodes in our shop, and cables not a problem. We have some that can 
carry thousands of amperes. And you need a fixture for holding the package 
and electrodes steadily with high pressure. One way would be to design the 
electrodes in a way that they make a circle around the feedtrue...one on 
each side. That would create a dense and well defined current flow.

I love experiments, will think it over.

Inge


----- Original Message ----- 
From: "Thayer, Wayne" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Wednesday, September 24, 2008 8:17 AM
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice


Hi Inge!

Nickel is pretty lossy, so you could possibly heat with electrical
energy.  Still lots of current required--probably on the order of
100A/mm of nickel.  Nickel doesn't conduct heat real well either, so you
would want to drive the current pretty close to where the solder needs
to be melted.  I'll bet a few days of playing with an arc welding power
supply would get you a process.  Or you could just use a car battery and
some jumper cables and see what happens!

Problem I see with this technique might be package warpage due to
differential coeff of expansion and the local heat, similar to problems
of using a torch, but the electrical would have much better control.

Wayne Thayer

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, September 24, 2008 10:46 AM
To: [log in to unmask]
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice

Mike,

THAT was new to me! Good start, I'd say, many thanks. Hope our machine
can manage 260 C.

Inge

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Mike Sewell
Sent: den 24 september 2008 16:33
To: [log in to unmask]
Subject: Re: [TN] Soldering SMA to heavy RF packages, need advice

Inge,

Galden makes fluids that go to 260C...

http://www.solvaysolexis.com/static/wma/pdf/9/7/7/0/Galden%20VPS.pdf

Mike

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Hernefjord Ingemar
Sent: Wednesday, September 24, 2008 9:26 AM
To: [log in to unmask]
Subject: [TN] Soldering SMA to heavy RF packages, need advice

 TNetters godday.

Target is very large metal packages with bright nickel finish. Imagine
soldering hermetic feedtrues. Nickel needs higher temperature and longer
exposure time than copper, silver, gold and other metals. Vapour phase
soldering is maximum 218 Centigrades, which I believe is not high
enough. Iron soldering is not practical for launches. IR oven could be
an idea if we add protection gas. Hot gas stations (Nitrogen)seem to be
too lame. Resistance soldering not tested, unknown for SMA. Torch heard
of, ought to be impractical, will burn flux and miscolor package. Laser
soldering not practised.

Anyone out there with experience from this kind of soldering?

Inge

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing
per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

This e-mail and any files transmitted with it may be proprietary and are 
intended solely for the use of the individual or entity to whom they are 
addressed. If you have received this e-mail in error please notify the 
sender.
Please note that any views or opinions presented in this e-mail are solely 
those of the author and do not necessarily represent those of ITT 
Corporation. The recipient should check this e-mail and any attachments for 
the presence of viruses. ITT accepts no liability for any damage caused by 
any virus transmitted by this e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2