Hello,
I'll try sending this one out again since I didn't see any responses
last week.
On all of our PCB fab drawings there is a specification which reads:
Land/Hole fabrication allowance shall be 0.012.
What does this spec mean?
Our PCB designer and two board houses I've spoken to do not know what
this spec is referring to. Our PCB designer states that this wording
can be found in IPC-D-325A, Documentation Requirements for Printed
Boards, in an example fab drawing.
Steve Hawn
Precision Digital Images
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|