TECHNET Archives

April 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, "Jeremias, Michael" <[log in to unmask]>
Date:
Thu, 1 Apr 2010 21:28:45 -0500
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Content-Transfer-Encoding:
quoted-printable
Subject:
From:
"David D. Hillman" <[log in to unmask]>
X-cc:
In-Reply-To:
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (314 lines)
Hi Michael! Here is my best guess at what "might" work in terms of getting 
a leaded component to have useable solderability after 30 years of storage 
( I say "might" because the only data I have is in the 5-10 year range). 
First and foremost, you need sufficient surface finish thickness such that 
room temperature diffusion will not cause the base lead alloy (i.e. copper 
or alloy 42) to diffuse thru the surface finish. If you can tackle that 
issue then you just need to prevent surface finish oxidation. If you seal 
the components in moisture proof package (aka MSL type packaging) using 
argon as a backfill gas and then  store the sealed bags in a 
humidity/temperature controlled environment, you might have a chance. You 
will be able to achieve at least 5-8 years of storage depending on the 
specific component surface finish you are dealing with. This is not a 
cheap procedure to use. Good Luck.

Dave Hillman
Rockwell Collins
[log in to unmask]




"Jeremias, Michael" <[log in to unmask]> 
Sent by: TechNet <[log in to unmask]>
03/26/2010 06:21 AM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
"Jeremias, Michael" <[log in to unmask]>


To
[log in to unmask]
cc

Subject
[TN] Long term Shelf life of electronic components






 Hi partners,

for long term storage and extended  shelf up to  30  Years  of  Plastic 
BGAs J-STD-033 is  very  valuable.

We need  long term shelf life  20....30 Years  for  Flash PROMS and  Flash 
Memories.

1. Do  You  know  Humidity seal bag materials  for longer  shelf life than 
12 months  e.g  5  Years or more?

2. Do You  know test procedures to be  done before  longterm storage of 
the iece parts?

3. Do  You  know  standrds  for  storge conditions  and  packing 
materials?

Thanks in advance for Any helpful answer 

Michael Jeremias 
 
-----Ursprüngliche Nachricht-----
Von: TechNet [mailto:[log in to unmask]] Im Auftrag von Bev Christian
Gesendet: Freitag, 26. März 2010 11:21
An: [log in to unmask]
Betreff: Re: [TN] Need some opinions

Inge,
What is a schrecklich photo?
Bev

----- Original Message -----
From: Inge <[log in to unmask]>
To: Bev Christian; [log in to unmask] <[log in to unmask]>
Sent: Fri Mar 26 03:11:06 2010
Subject: Re: [TN] Need some opinions

Bev,

The purpose of lead finish, either it is tinned or gold plated or silver 
plated, is not only to make the leads solderable, but also to protect the 
bulk material from corrosion.  A Kovar leg that is not 100% covered will 
be attacked and can corrode to the degree that the whole component falls 
off. 
If the leads are bent after tinning, there is still more risk of problems. 

So, of course negative wetting is something that the quality responsible 
must consider as a high priority case.  If you are interested, and if I 
can find, I can send some schrecklich photos to you.

Inge




--------------------------------------------------
From: "Bev Christian" <[log in to unmask]>
Sent: den 25 March 2010 18:58
To: <[log in to unmask]>
Subject: Re: [TN] Need some opinions

> Steve,
> Gull wings.
>
> Yes, cheap, cheap cheap!
>
> Bev
>
> ----- Original Message -----
> From: TechNet <[log in to unmask]>
> To: [log in to unmask] <[log in to unmask]>
> Sent: Thu Mar 25 21:49:18 2010
> Subject: Re: [TN] Need some opinions
>
> Hi Bev,
>
> Don't leave us hanging, what components are you seeing that with? I'd 
like
> to have a "heads-up".
>
> This begs the question, why do you think they are doing that? Are things
> getting so tight that they're trying to pinch a penny by reducing 
plating
> coverage? Hmmmm...
>
> Steve
>
> ----- Original Message ----- 
> From: "Bev Christian" <[log in to unmask]>
> To: <[log in to unmask]>
> Sent: Thursday, March 25, 2010 9:08 PM
> Subject: [TN] Need some opinions
>
>
>> Technetters,
>> It seems that more and more component suppliers are not plating their
>> leads
>> all the way up to the component body. In fact some are getting 
downright
>> skimpy and only plating to the bottom bend, never mind the upper one. 
If
>> you
>> put down a lot of solder paste you end up with a bulbous joint, a 
>> negative
>> wetting angle and a stress concentration point. If you put down less 
>> paste
>> and have a co-planarity issue, then you have the potential for opens. 
>> The
>> other option of course is getting the supplier to plate higher up the
>> leads.
>>
>> Question: would you consider the condition of the formation of the
>> negative
>> wetting angles a failure during process qualification?
>>
>> Bev
>> RIM
>>
>>
>> ______________________________________________________________________
>> This email has been scanned by the MessageLabs Email Security System.
>> For more information please contact helpdesk at x2960 or 
[log in to unmask]
>> ______________________________________________________________________
>>
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0
>> To unsubscribe, send a message to [log in to unmask] with following text 
in
>> the BODY (NOT the subject field): SIGNOFF Technet
>> To temporarily halt or (re-start) delivery of Technet send e-mail to
>> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
>> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives
>> Please visit IPC web site 
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
>> for additional information, or contact Keach Sasamori at [log in to unmask] 

>> or
>> 847-615-7100 ext.2815
>> ----------------------------------------------------- 
>
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or 
> 847-615-7100 ext.2815
> -----------------------------------------------------
>
> ---------------------------------------------------------------------
> This transmission (including any attachments) may contain confidential 
> information, privileged material (including material protected by the 
> solicitor-client or other applicable privileges), or constitute 
non-public 
> information. Any use of this information by anyone other than the 
intended 
> recipient is prohibited. If you have received this transmission in 
error, 
> please immediately reply to the sender and delete this information from 
> your system. Use, dissemination, distribution, or reproduction of this 
> transmission by unintended recipients is not authorized and may be 
> unlawful.
>
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
[log in to unmask]
> ______________________________________________________________________
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0
> To unsubscribe, send a message to [log in to unmask] with following text 
in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to 
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to 
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: 
http://listserv.ipc.org/archives
> Please visit IPC web site 
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at [log in to unmask] 
or 
> 847-615-7100 ext.2815
> ----------------------------------------------------- 


---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute non-public 
information. Any use of this information by anyone other than the intended 
recipient is prohibited. If you have received this transmission in error, 
please immediately reply to the sender and delete this information from 
your system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be 
unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask] or 
847-615-7100 ext.2815
-----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2