Information I've read indicates there is a good possibility of the leaded
solder on the components diffusing into the lead free solder, creating a new
alloy which may behave differently than intended. This may be something
else to consider in addition to temperature.
Shean R. Dalton
Austin American Technologies
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Balasubramanian
Krishnan
Sent: Friday, June 04, 2004 8:13 AM
To: [log in to unmask]
Subject: [TN] Mixed assembly of ROHS & Non ROHS components
Dear Experts,
Is it possible to use some normal components (with lead) along with
lead free components in the same PCBA. Since the tempertaure requirement of
lead free components is higher will it affect the normal components? Or is
it possible to assemble normal components first and then lead free next in
two steps. Please guide me.
Sincerely
K.Balasubramanian
Sr.Engineer, Hardware.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------
|
|
|