TECHNET Archives

March 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Michael Forrester <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Tue, 14 Mar 2006 06:49:26 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
I am currently having a soldering issue with a Samtec SMT connector.  We
are seeing cracks in the solder joints
on the inner row.  The lead of the connector is only the butt end of the
connector pin that makes contact to the PCB.
I have included some specifications:

(Embedded image moved to file: pic18467.jpg)
The lead pulls out of the solder joint very easily in the length direction.
It leaves a crater in the solder deposit.  The
solder is fully wetted to the pad and pin.  If I bend the pin parallel to
the length it comes out of the joint like the joint
is butter.  The pin is gold plated and the board surface is OSP.  I would
think that the PAD should pull up before the
solder joint fails?  Any ideas or help would be greatly appreciated.

Thank You,

Mike Forrester


PS.  Detail pictures enclosed:

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
(See attached file: Samtec J1 Connector.xls)

ATOM RSS1 RSS2