Hi Technetters:
I am looking for a prepreg which can be laminated to 0.002' thickness and
the resultant can withstand 10 cycles of 2 hours temperature soak at 200C.
I wonder if high Tg epoxy material can withstand the condition. If so, what
is the laminate Tg range I have to look for. If epoxy can not meet the
requirement, please advise me the right material to use.
Thanks in advance.
M. C. Chu
CSS Asia Co., Ltd.
Tel: 82-2-523-8810
Fax: 82-2-523-1483
E-Mail: [log in to unmask]
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################
|
|
|