TECHNET Archives

July 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Kathy Kuhlow <[log in to unmask]>
Date:
Thu, 19 Jul 2001 09:46:24 -0500
Content-Type:
multipart/mixed; boundary="=_227842D5.187915AD"
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Kathy Kuhlow <[log in to unmask]>
Parts/Attachments:
text/plain (466 bytes) , TEXT.htm (868 bytes)
Thanks to all who responded to my questions regarding white residues in conformal coating. 

Just an update:  To prove beyond a doubt that the issue was caused by humidity a small sample of the assemblies were sprayed and then put into an air conditioned room to dry.  Those samples look great.  Now on to discuss why the supplier didn't know this would be an issue and didn't control their process.  

I guess I will get out of the office for awhile.  

Kathy 



<!DOCTYPE HTML PUBLIC "-//W3C//DTD HTML 4.0 Transitional//EN"> <HTML><HEAD> <META content="text/html; charset=iso-8859-1" http-equiv=Content-Type> <META content="MSHTML 5.00.2614.3500" name=GENERATOR></HEAD> <BODY style="FONT: 10pt Haettenschweiler; MARGIN-LEFT: 2px; MARGIN-TOP: 2px"> <DIV>Thanks to all who responded to my questions regarding white residues in conformal coating.&nbsp;</DIV> <DIV>&nbsp;</DIV> <DIV>Just an update:&nbsp; To prove beyond a doubt that the issue was caused by humidity a small sample of the assemblies were sprayed and then put into an air conditioned room to dry.&nbsp; Those samples look great.&nbsp; Now on to discuss why the supplier didn't know this would be an issue and didn't control their process.&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>I guess I will get out of the office for awhile.&nbsp; </DIV> <DIV>&nbsp;</DIV> <DIV>Kathy </DIV></BODY></HTML>