TECHNET Archives

March 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
Subject:
From:
David Anderson <[log in to unmask]>
Date:
Sat, 21 Mar 1998 16:09:49 -0600
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Anderson <[log in to unmask]>
Parts/Attachments:
text/plain (33 lines)
Plating from small volume baths is definitely possible, but I think that
one thing to watch out for when plating out of a beaker is that the metal
content of the baths can change quickly due to the small volumes of the
solutions.  As you plate onto your work piece, metal (as well as other
things) is consumed in the bath, which may change the plating rate,
quality, etc.

Perhaps I have just been unlucky enough to have fussy plating makeups in
the past, but it was a noticeable effect in the some of the chemistries I
have worked with if the parts are large enough and the bath is small
enough.

This may not be an issue depending on the size of the beakers, size of the
work piece, thickness of the plating, etc., but may be something to think
about.

Dave Anderson
Medtronic, Inc.

Opinions stated are my own, and not necessarily those of my employer.

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################


ATOM RSS1 RSS2