TECHNET Archives

February 2007

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Douglas O. Pauls" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 2 Feb 2007 11:47:23 -0600
Content-Type:
text/plain
Parts/Attachments:
text/plain (86 lines)
Steve,
That appears to me to be tape that has not been removed from the board,
rather than any residues from the adhesive.  I have used the Humiseal tape
with success and have not seen these kinds of failures when the tape is
removed while the coating is wet.  If you allow the coating to dry or be
tack free, then you get these kinds of problems.  I would expect you to
have the same problem with other kinds of tape.

Doug Pauls



                                                                           
             Steve Gregory                                                 
             <SGregory@OAIELEC                                             
             TRONICS.COM>                                               To 
             Sent by: TechNet          [log in to unmask]                     
             <[log in to unmask]>                                          cc 
                                                                           
                                                                   Subject 
             02/02/2007 11:30          [TN] Humiseal Masking Tape          
             AM                        Residues...                         
                                                                           
                                                                           
             Please respond to                                             
              TechNet E-Mail                                               
                   Forum                                                   
             <[log in to unmask]>                                             
             ; Please respond                                              
                    to                                                     
               Steve Gregory                                               
             <SGregory@OAIELEC                                             
               TRONICS.COM>                                                
                                                                           
                                                                           




Hi All!

I have a conformal coat masking problem too along with KennyB. We're
getting residues from the Humiseal tape we're using when we remove the
tape.

We're coating the boards with 1B31, and we don't bake the boards with
the tape on. We take the tape off right after we spray the board. Check
out:

http://stevezeva.homestead.com/files/Tape_Residues.jpg

I've not had this problem with Humiseal tape before. Our customer is
rejecting the boards and it is quite time consuming to remove these
residues.

I've got a call into Humiseal to see if they can help. Do any of you use
any other tape for masking that doesn't leave residues?

Have a great Friday!

-Steve Gregory-

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2