I don't hink you'll be in trouble. The bake-out requirements are determined
by the MSD Category, and if you have the category number (or 'level') you
can get the times and temperatures from J-STD-020 or J-STD 033.
Peter
Andre Leclair <[log in to unmask]> 12/07/2002 01:22 AM
Sent by: TechNet <[log in to unmask]>
Please respond to "TechNet E-Mail Forum."; Please respond to Andre Leclair
To: [log in to unmask]
cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Subject: [TN] Moisture Sensitive ( Not ICs)
Hi All
We have just started receiving some components for a new customer job and
noted that they were moisture Sensitive, these were some Caps and some
LEDS.
Has any one seen these before??
There was no information on the packaging other then the Level #.
Bake and process requirements were left blank.
Would I be asking for trouble if I followed the generic requirements for
the specific levels of the devices?
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
[This e-mail is confidential and may also be privileged. If you are not the
intended recipient, please delete it and notify us immediately; you should
not copy or use it for any purpose, nor disclose its contents to any other
person. Thank you.]
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|