The easiest (and correct) way is to take a quick analysis (like EDS).
------Original Message------
From: Ashok Dhawan
Sender: TechNet
To: [log in to unmask]
ReplyTo: TechNet E-Mail Forum
ReplyTo: Ashok Dhawan
Subject: [TN] Black material under plating
Sent: Aug 31, 2010 18:17
Anyone encountered black coating like material under plating of heatsink ?
The package is TO 220. Upon desoldering the package or plying off the board
with a nose plier, it sheared off at plating. A portion of plating stayed on the
board while remaining on heatsink plate. The surface on parts' heatsink where
plating peeled off is black in color. On scratching with sharp tool, it appears to
have copper under.
The surface is tin lead plated. Any guesses what this black surface could be ?
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
Vladimir
SENTEC Testing Laboratory Inc.
11 Canadian Road, Unit 7.
Scarborough, ON M1R 5G1
Tel: (416) 899-1882
Fax: (905) 882-8812
www.sentec.ca
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|