At 08:28 21/07/98 +0300, you wrote:
>You could try AlphaLevel.
Could be so kind and explain to the forum , how AlfaLevel ( alternative
finishing for soldering ) will fix bowed boards ??? If it works in this way
, this is really great product .
>
>[log in to unmask] wrote:
>
>> Technetters.
>> We are manufacturing multilayer printed circuit boards.
>> One of our customers request us to make 6 layer memory module
>> board(7"X6.3"X0.05"t) of which bow tolerance is Max 0.30%.
>> It's very tough job.
>> Our 1st yield for that board is lower than 80%.
>> Lamination stack height, heating rate, cooling rate, cushion material, layup
>> construction, coppper balance, baking....
>> These parameters which I thought related with flatteness were tested many
>> times. But we still see bowed boards(Max 0.70%).
>> I will make every effort to make SUPER FLAT BOARD.
>> Any advice would be appreciated.
>> Thanks in advance.
>> Herold Green
>> ----------------------------------
>>
>> -----------------------------------------------------------
>> EasyPost - the FREE web based email service from EasySpace
>> Visit http://www.easyspace.com for the best deals on
>> virtual servers - just US$ 8.50 /month for 100 Meg webspace
>> with your domain name and Frontpage 98 extenions.
>> ----------------------------------------------------------
>>
>> ################################################################
>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>> ################################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>> To subscribe: SUBSCRIBE TechNet <your full name>
>> To unsubscribe: SIGNOFF TechNet
>> ################################################################
>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>> ################################################################
>
>
>
>--
>Jacob Mozel
>11 Hakalanit St
>44280 Kfar Saba, Israel
>Tel: +972 9 7425871
>Fax: +972 9 7424089
>e-mail: <[log in to unmask]
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
Edward Szpruch
Eltek Ltd - Israel
Tel 972 3 9395050
Fax 972 3 9309581
E-mail : [log in to unmask]
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|