TECHNET Archives

December 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
"West, Jim" <[log in to unmask]>
Date:
Thu, 16 Dec 1999 11:46:49 -0800
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Brian Stumm <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii
From:
Brian Stumm <[log in to unmask]>
Parts/Attachments:
text/plain (61 lines)
Jim,

In addition to my other post...

Once you have verified profiler calibration use the profiler to verify oven
calibration. Attach thermocouples to a board or something so that the thermocouples are
in the open air (tape them so the stick up off the board) and run through oven. As it
passes through each zone it will tell you that zones temperature, compare that to the
actual zone temperature as reported by the systems software. The frequency at which you
check your oven conveyor speed calibration and zone temperature accuracy depends on how
much you use it but I would verify at least every couple of months (or when you suspect
a change in your process). Check individual processes more frequently using your test
profiling board (which is an accurate representation of the product you are building).
I would test my profile recipes every couple of weeks at least.

Brian Stumm
ETS, Inc.

"West, Jim" wrote:

> Hi,
>
> Do you have a calibration program set-up for your re-flow oven?
>
> How do you verify the temperature and conveyor speed?
>
> What is the frequency of checking re-flow ovens?
>
> All the questions are ISO related.
>
> Thanks,
> Jim
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
> information.
> If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
> 847-509-9700 ext.5365
> ##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2