REF message
Date:    Mon, 19 Jan 1998 14:19:54 -0500
From:    David Tyler <[log in to unmask]>
BeCu can be made into flex circuit material, but as far as I know it's not
commercially available. The problems in the past have been that the Be
suppliers do not make the foil in the typical thickness needed, and do not
apply the typical adhesion treatments used for flex. The flex materials
manufacture had to get the foil rolled thinner, and have it treated by
several third parties.

Most recent applications have called for it because of the mechanical
properties. These were switched to materials like Olin's Alloy 7025 that
has "good enough" mechanical performance, while maintaining much more of
its conductivity than BeCu, It's also commercially available in the right
configuration.

There may also be some concern about the toxicity of Be in processing,
primarily encountered in machining operations like drill and route, where
metallic dust can be generated.

Andy Magee
V.P. of Opns
Mound Flexible Circuits
[log in to unmask]
(937) 865-4232

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
##############################################################

ATOM RSS1 RSS2