Hi Technets !
We started to work with our new line of electroless Ni-Au finishing. We have
some problems , that seems to be similar to those , that were discussed 3
weeks ago in the net . We observed several phenomenas, that are confusing us :
1 ) Usually , we are adding to working basket brushed , double sided pannels
just to have enough surface , as reguested by loading factor . I happend ,
that one of those pieces got Nickel on one side , while the the second side
was vitrually not plated . Production boars were plated correctly .
2 )  We observed , that some pads on MLB are not plated .We found out , that
they are electrically connected .
3 ) As far as  we know , double sided boards are not affected by " selective
non-plating "

We have a filling , that this problem is somehow connected with the network
on the board . We don`t know , how to define the reasons and how to overcome
the problems .

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2