Larry:
If you havn't already, you should look at the standoff height, or space
undernieth of the problem component packages. SOL's and other SMT
packages have more standoff and will require a higher adhesive deposition to
get a good bond between component and PCB. If that is the issue, you may
have to go to a thicker stencil to get the higher adhesive deposition.
Kelly
---------------------------------------------------