And of course for proof of concept you will have to perform several trials
.......................
John
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------
-----Original Message-----
From: Barmuta, Mike [mailto:[log in to unmask]]
Sent: Friday, October 21, 2005 2:28 PM
To: 'John Burke'; Barmuta, Mike; 'TechNet E-Mail Forum'
Subject: RE: [TN] (NTC)Removing oxide from silver flakes.
John: I've found you need to rinse and strain at least twice sometimes more.
It really depends on the number of flakes you've worked with that week and
how tarnished they were.
Mike Barmuta
-----Original Message-----
From: John Burke [mailto:[log in to unmask]]
Sent: Friday, October 21, 2005 1:56 PM
To: 'Barmuta, Mike'; 'TechNet E-Mail Forum'; John Burke
Subject: RE: [TN] Removing oxide from silver flakes.
So let me get this right, you take your rinsed silver flake, add 180 proof
alchohol (shaken not stirred), drain the alcohol into a suitable vessel
(martini glass??)and then what add vermouth?.
So presumably to have to do this several times??
John
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------
-----Original Message-----
From: Barmuta, Mike [ mailto:[log in to unmask]
<mailto:[log in to unmask]> ]
Sent: Friday, October 21, 2005 1:50 PM
To: 'TechNet E-Mail Forum'; 'John Burke'
Cc: Barmuta, Mike
Subject: RE: [TN] Removing oxide from silver flakes.
Actually John you're not far off in your Bud comment. After final DI rinse
follow with two alcohol rinses. One to displace the water and the second to
provide a fast evaporating rinse media when placed in the oven. Use a good
grade, electronic or above isopropyl alcohol. Better yet 190 proof ethanol
and start the weekend out right.
Mike Barmuta
-----Original Message-----
From: TechNet [ mailto:[log in to unmask] <mailto:[log in to unmask]> ]On Behalf
Of John Burke
Sent: Friday, October 21, 2005 1:41 PM
To: [log in to unmask]
Subject: Re: [TN] Removing oxide from silver flakes.
I guess havng removed it, the rinsing and drying wil have to be carefully
addressed to avoid re-oxodising the silver, maybe several agitated rinses in
DI water followed by heating in a nitrogen purged batch oven.
As for the rinsing material as it is Friday my suggestion for an alternate
is Bud light since it is absolutely tasteless/odorless...........8-)
John
------------------------------------
Avanex
John Burke
Senior Manager RoHS Compliance
[log in to unmask]
40919 Encyclopedia Circle
Fremont
CA 94538
tel: 510 897 4250
fax: 510 979 0189
mobile: 510 676 6312
------------------------------------
-----Original Message-----
From: TechNet [ mailto:[log in to unmask] <mailto:[log in to unmask]> ]On Behalf
Of R Sedlak
Sent: Friday, October 21, 2005 1:33 PM
To: [log in to unmask]
Subject: Re: [TN] Removing oxide from silver flakes.
In the US, I would send you down to your local supermarket to buy a bottle
of silver tarnish remover....
Another way to do this, depending on your situation is to find a mildly
alkaline detergent solution, and pour the silver flakes on to a piece of
aluminum foil, and immerse in the mildly alkaline detergent solution... this
will reduce the Silver oxide to silver metal...
Good luck, let us know if it worked.
Rudy Sedlak
RD Chemical Company
Syed Sajid Ahmad <[log in to unmask]> wrote:
Any help on getting rid of oxide on silver flakes will be appreciated.
Thanks.
Syed.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
Yahoo! FareChase - Search multiple travel sites in one click.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
<http://listserv.ipc.org/archives>
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
<http://www.ipc.org/contentpage.asp?Pageid=4.3.16>
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|