TECHNET Archives

August 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Graham Naisbitt <[log in to unmask]>
Date:
Tue, 10 Aug 2010 16:10:31 +0100
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "Fox, Ian" <[log in to unmask]>
Subject:
From:
"Fox, Ian" <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (315 lines)
You can get your own back down at NPL in september. I'll put a big book
down the back of me trousers........

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
Sent: 10 August 2010 15:45
To: [log in to unmask]
Subject: Re: [TN] blumpy (codeposited organics)

Oi! Enough of that Ian - I do not wish to disabuse Techies knowledge of
me....

Graham N

On 10 Aug 2010, at 13:53, Fox, Ian wrote:

> Oh what a sheltered life you've led Steve. Now Graham on the other 
> hand...............
> 
> Regards
> Ian
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Steve Gregory
> Sent: 10 August 2010 13:28
> To: [log in to unmask]
> Subject: Re: [TN] blumpy (codeposited organics)
> 
> Like Guy, I had to look it up since Graham pointed it out, and I 
> didn't think it was a real word.
> 
> I should have never looked it up. I could have gone all day without 
> knowing what that meant.
> 
> Steve
> 
> -----Original Message-----
> From: TechNet [mailto:[log in to unmask]] On Behalf Of Graham Naisbitt
> Sent: Tuesday, August 10, 2010 5:59 AM
> To: [log in to unmask]
> Subject: Re: [TN] blumpy (codeposited organics)
> 
> Ahem. Please do NOT use the term "Blumpy" - it has a meaning in the 
> slang dictionary that you REALLY don't want to know!
> 
> Having taken a look at Chris's photo, I think the correct term might 
> be "Clumpy - having or showing a tendency to form clumps"
> 
> Clump = as a noun: a compacted mass or lump of.... as a verb: to form 
> into a mass or clump
> 
> Graham N
> 
> 
> On 6 Aug 2010, at 23:23, Chris Mahanna wrote:
> 
>> I'm not giving up the secret, but it is the same way that you use a
> metallograph to tell which way the train was moving.
>> 
>> I have loose parts and they are definitely not Ni/Pd/Au.  Nor is 
>> there
> 
>> any
> indication of insufficient heat on the surrounding parts.  Actually my

> first response to the customer was incomplete coalescence due to lack 
> of flux activity.  But he didn't like that answer, because he knew it 
> was only related to that batch of parts.  So, I went back and looked 
> up Rich Kraszewski's recipe for smoking out organics.
>> At the moment, I'd say there is a good chance they are counterfeit 
>> parts,
> but they might just be really old and contaminated...?
>> Anyhow, since no one objected, I'm going to use the term blumpy in 
>> the
> report.
>> 
>> Have a great weekend everyone.
>> 
>> Chris
>> 
>> From: [log in to unmask] 
>> [mailto:[log in to unmask]]
>> Sent: Friday, August 06, 2010 4:27 PM
>> To: TechNet E-Mail Forum; Chris Mahanna
>> Subject: Re: [TN] blumpy (codeposited organics)
>> 
>> 
>> I'm just curious how Chris got a freight train under a
> microscope...............
>> 
>> Doug Pauls
>> 
>> Chris Mahanna <[log in to unmask]>
>> Sent by: TechNet <[log in to unmask]>
>> 
>> 08/06/2010 12:39 PM
>> Please respond to
>> TechNet E-Mail Forum <[log in to unmask]>; Please respond to Chris 
>> Mahanna <[log in to unmask]>
>> 
>> 
>> To
>> 
>> [log in to unmask]
>> 
>> cc
>> 
>> Subject
>> 
>> [TN] blumpy (codeposited organics)
>> 
>> 
>> 
>> 
>> 
>> 
>> 
>> So a customer has the blumpies.  The hand (dry) solder melt-front 
>> smokes
> like a freight train under the microscope.
>> 
>> 
>> 
>> My questions are:
>> 
>> 
>> 
>> Have we really coined "blumpy"? and
>> If it wets and forms proper fillets, is it conformant?
>> 
>> Thanks!
>> Chris
>> 
>> Click here<https://robisan.sharefile.com/d-s8f0852004d94e529> to 
>> download
> attachments.
>> 
>> _____________________________________________________________________
>> _ This email has been scanned by the MessageLabs Email Security 
>> System.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

>> unsubscribe, send a message to [log in to unmask] with following text 
>> in
> 
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt

>> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
>> 
>> _____________________________________________________________________
>> _ This email has been scanned by the MessageLabs Email Security 
>> System.
>> For more information please contact helpdesk at x2960 or 
>> [log in to unmask] 
>> _____________________________________________________________________
>> _
>> 
>> ---------------------------------------------------
>> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To

>> unsubscribe, send a message to [log in to unmask] with following text 
>> in
> 
>> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt

>> or (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL)
>> To receive ONE mailing per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
>> Search the archives of previous posts at: 
>> http://listserv.ipc.org/archives Please visit IPC web site
>> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
>> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or
> (re-start) delivery of Technet send e-mail to
> [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing 
> per day of all the posts: send e-mail to
> [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at:
> http://listserv.ipc.org/archives Please visit IPC web site
> http://www.ipc.org/contentpage.asp?Pageid=4.3.16
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or
> (re-start) delivery of Technet send e-mail to [log in to unmask]: SET 
> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please

> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 
> ----------------------------------------------------------------------
> ---- This message (and any attachment) is confidential and is intended

> for the named recipient only.
> If you receive it in error please e-mail back the sender and
permanently delete the original message and any copies.
> Rolls-Royce Goodrich Engine Control Systems Limited.
> Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ.
> Registered in England No. 06686268.
> ----------------------------------------------------------------------
> ----
> 
> ______________________________________________________________________
> This email has been scanned by the MessageLabs Email Security System.
> For more information please contact helpdesk at x2960 or 
> [log in to unmask] 
> ______________________________________________________________________
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 15.0 To 
> unsubscribe, send a message to [log in to unmask] with following text in

> the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt 
> or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET

> Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the 
> posts: send e-mail to [log in to unmask]: SET Technet Digest Search the 
> archives of previous posts at: http://listserv.ipc.org/archives Please

> visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
> for additional information, or contact Keach Sasamori at 
> [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------


______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or
[log in to unmask]
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0 To
unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the
posts: send e-mail to [log in to unmask]: SET Technet Digest Search the
archives of previous posts at: http://listserv.ipc.org/archives Please
visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for
additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

--------------------------------------------------------------------------
This message (and any attachment) is confidential and is intended for the named recipient only.
If you receive it in error please e-mail back the sender and permanently delete the original message and any copies.
Rolls-Royce Goodrich Engine Control Systems Limited.
Registered Office: Moor Lane, PO Box 31, Derby, DE24 8BJ.
Registered in England No. 06686268.
--------------------------------------------------------------------------

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2