TECHNET Archives

April 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=US-ASCII
X-To:
George Gerberick <[log in to unmask]>
Date:
Wed, 21 Apr 1999 07:37:55 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
From:
Andy Slade <[log in to unmask]>
Content-Transfer-Encoding:
7bit
Sender:
Parts/Attachments:
text/plain (86 lines)
     Hi Dennis,

     Assuming that the remaining area is bare copper, you can overplate the
     entire pattern with tin/lead, then reimage to protect the features you
     want tin/lead, then solder strip the unprotected areas (selective
     solder strip).  Strip your resist, soldermask over the bare copper,
     then reflow.

     Hope this helps...Andy


______________________________ Reply Separator _________________________________
Subject: Re: [TN] Electrolytic plating on isolated areas or an altern
Author:  George Gerberick <[log in to unmask]> at smtplink-hadco
Date:    04/20/99 2:42 PM


What is on the balance of the circuitry? Can you electrolytic plate, dry film
mask and plate again in those
isolated areas before etch?

[log in to unmask] wrote:

> From: Dennis J Fall@TFT on 04/20/99 03:06 PM
>
> To:   [log in to unmask]
> cc:
> Subject:  Electrolytic plating on isolated areas or an alternative
>
> I have been pulling my hair out trying to figure out how to electroplate
> solder onto isolated areas (land pads, etc.).  I have also been trying to
> come up with other ways to do this (immersion, etc.).  I basically need
> about 5 ?m (0.2 mils) of solder.  Does anyone have any great ideas???????
>
> Thank You,
>
> Dennis Fall                        P: 507-625-8445 x17
>
> Engineer                           F: 507-625-3523
>
> Thin Film Technology Corporation         mailto:[log in to unmask]
>
> 1980 Commerce Drive                http://www.thin-film.com
>
> North Mankato, MN 56003-1702
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
> To subscribe:   SUBSCRIBE TechNet <your full name>
> To unsubscribe:   SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
> ################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text
in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for
additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700
ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2