TECHNET Archives

May 2013

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Steve Gregory <[log in to unmask]>
Date:
Fri, 17 May 2013 09:25:06 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, "lduso - Diamond-MT.com" <[log in to unmask]>
Subject:
From:
"lduso - Diamond-MT.com" <[log in to unmask]>
Message-ID:
In-Reply-To:
<E7D3176B82F34EBAB196CCD0BEA04714@stephenPC>
Content-Type:
text/plain; charset="ISO-8859-1"
MIME-Version:
1.0
Parts/Attachments:
text/plain (49 lines)
Tough to put into practice. With masking you want to get the masking
material off before the coating has completely cured to minimize lifting
and peeling. The washing machine could damage that uncured coating. Plus
the coating is covering the masking so the water will not touch the masking
to dissolve it until the coating is removed from it first. I tried it with
parylene and we had to pick holes in the film so the water could access the
masking then go back and trim off the excess after the masking dissolved
and we were left with a "tent" of film

Re-usable boots are ideal but could be costly when you have many different
style/sizes of connectors.

Like we tell all our customers, cheapest way to coat something is leave off
all the connectors!!

Lloyd Duso
Diamond-MT
Plant Manager
(814) 535-3505
www.Diamond-mt.com


On Fri, May 17, 2013 at 9:08 AM, Steve Gregory <
[log in to unmask]> wrote:

> Morning all,
>
> Continuing on with the masking thread, I know Techspray has a water
> soluble mask that is supposed to be compatible with closed-loop water
> treatment systems, are there any others out there?
>
> Any pros/cons of using them?
>
> As always, thanks in advance!
>
> Steve
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2