Here ya go!
IPC-A-600 Rev C 2.10.1.2 Conductor Spacing
Target Condition - Class 1, 2, 3
Conductor spacing meets dimensional requirements of the procurement
documentation.
Acceptable - Class 3
Any combination of edge roughness, copper spikes, etc., that does not reduce
the specified minimum conductor spacing by more than 20% in isolated areas.
Acceptable - Class 1, 2
Any combination of edge roughness, copper spikes, etc., that does not reduce
the specified minimum conductor spacing by more than 30% in isolated areas.
Hans
~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Process Engineer
Toppan Electronics, Inc.
770 Miramar Road
San Diego, CA 92126
(858) 695 - 2222 ext. 241
(858) 695 - 6823 fax
[log in to unmask]
-----Original Message-----
From: Brian Hall [mailto:[log in to unmask]]
Sent: Tuesday, November 07, 2000 5:31 AM
To: [log in to unmask]
Subject: [TN] spec on stray copper
Does anyone know if there is a spec on the size a particle of stray copper
can't exceed on the outer layer of a circuit board?
Thanks
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|