At 14:26 28.05.98 -0500, you wrote:
>What is FR1 and how does it differ from FR4?
Just my topic!
FR1 is very similar to FR2, both are UL94-V0, both use a phenolic resin as
binder. The only difference to FR2 is the phenolic resin, which is a
different type. FR1 is mainly cold punchable and has a slightly better
operation temperatur. Therefore, many laminate maker which produce FR1 do
not produce FR2. Also, FR1 prices are the same as FR2.
I consider myself as having some knowledge about laminates - still, I can't
tell the difference between FR1 + FR2.
FR4 is a glass epoxy material and is completly different.
Jens Behrens
Want to know more about laminate? http://www.felsweb.com/lam_faq.htm
Laminate FAQ
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
>To subscribe: SUBSCRIBE TechNet <your full name>
>To unsubscribe: SIGNOFF TechNet
>################################################################
>Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|