TECHNET Archives

May 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset="iso-8859-1"
Old-Return-Path:
Date:
Thu, 1 May 1997 12:42:06 -0700
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
From [log in to unmask] Fri May 2 09:
51:25 1997
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12380
X-Sender:
TO:
Return-Path:
<TechNet-request>
X-Status:
X-Loop:
Resent-Message-ID:
<"2u8oy2.0.SGB.A_EQp"@ipc>
Subject:
From:
Phil Bavaro <[log in to unmask]>
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wN1ad-000BjAC; Thu, 1 May 97 14:32 CDT
In-Reply-To:
Content-Transfer-Encoding:
quoted-printable
Message-Id:
<v03007804af8ea2448457@[129.46.191.125]>
Parts/Attachments:
text/plain (44 lines)
Our assemblies operate as high as 12 GHz with no problems over the last
five years of no clean assembly.

Phil
-----


At 12:07 PM -0400 4/30/97, Brian Bauer wrote:
>Hello,
>
>Does anyone have any information on the effect of no clean residues on RF.
>I am interested at what frequency interference begins (if any) and what type
>of device you are talking about ie. phine, radio etc..  I am interested in
>both PCB and Hybrid Thick Film (alumnia) applications. Also, is anyone using
>no cleans in the Gigahertz level - if so what level?
>
>Thanks
>
>Brian
>
>***************************************************************************
>* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
>***************************************************************************
>* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
>* with <subject: subscribe/unsubscribe> and no text in the body.          *
>***************************************************************************
>* If you are having a problem with the IPC TechNet forum please contact   *
>* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
>***************************************************************************



***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2