Hello All,
I am working with a customer to determine the optimal finished hole diameter
for press-fit connectors in a Gold finish PCB. The supplier's data sheet for
the connector specifies .024"+/-.002" HASL plated holes. We have learned
from experience that the connector insertion success rate is greatly
improved when using a slightly larger hole on a gold finish PCB since it is
less compliant with the connector pins then the soft HASL.
So far, the supplier has not given a recommendation on the diameter for
gold, so I am looking for other industry standards to validate our findings.
Any help would be greatly appreciated.
Dave Pahlas
Mfg Engineer
(208) 898-1072
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|