TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Matthew Park <[log in to unmask]>
Date:
Mon, 22 Mar 1999 12:21:01 -0800
Content-Type:
text/plain
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Matthew Park <[log in to unmask]>
Parts/Attachments:
text/plain (67 lines)
Mr. Brunker,

I done on/off studies of various plastic materials for the
application of squeegee blade for solder paste printing.  One
purpose of my study was to eliminate stencil wear that  you
mentioned using a metal blade such as a Transition Automation
Permalex metal squeegee, and at the same time to eliminate
the printing problem associated with using a polyurethane
rubber squeegee.

By using these materials, I had good success reducing stencil
wear significantly, and bringing printing quality to that of metal
squeegee.  Is this something you are looking for?  One major
factor of stencil wear  is due to uneven support of boards during
printing cycles.  Board-Lok support jigs from Transition
Automation provide even support and eliminate many printing
defects associated with double sided printing.

Regards
Matthew Park
Norsat International Inc.


>>> Edward Brunker <[log in to unmask]> March 18,
1999  2:38 am >>>
     Hi,
     Has anyone done any studies for the change of depth of
solder paste
     with wear on the stencil. Metal blade squeegees damage the
stencil
     over a period of time, yielding an uneven surface in the form of
     furrows in the direction of travel. Any uneveness in the stencil
is
     going to hold the blades that much further off the board giving
more
     solder paste.
     Any comments?
     Regards
     Edward Brunker

################################################################
TechNet E-Mail Forum provided as a free service by IPC using
LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to
[log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line
Services" section for additional information.
For technical support contact Hugo Scaramuzza at
[log in to unmask] or 847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2