TECHNET Archives

July 2015

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 3 Jul 2015 17:05:02 +0300
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Message-ID:
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
7bit
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
Well, Joyce, my first remark is exposing DVDs/VHS tapes to sunlight is a 
big mistake, especially in the greenhouse of a plastic case.
"Direct sunlight can harm VHS tapes

One of the most damaging environmental conditions that can degrade the 
longevity of a VHS tape is if it has been stored in direct sunlight. 
Direct sunlight dramatically reduces how long a VHS tape can last."
 From http://www.memoryhub.com/news/how-long-do-vhs-tapes-last/

The same can apply to  optical storage, especially R types.

I'm pretty sure that plastic degradation does not occur with a couple of 
minutes, or even hours, exposure to sunlight through a window which 
blocks UV. Personally, I see no objection to using bioplastics for 
packaging video records of any type and I would not shoot the 'engineer' 
who selected those plastics.

I take on board your point about recycling bioplastics, something that I 
haven't considered. However, I must ask that, if they become a powder at 
the drop of a hat, how can you recycle them?

Best regards,

Brian.

On 03/07/2015 16:01, Joyce Koo wrote:
> I just have to vent: some of my VHS and DVD cover plastic overlay turn
> into dust upon expose to the sunlight.  Who is the engineer to select bio
> degradable plastic as cover overlay should get shot at... dealt with a
> plastic bag that holding my design book last year with similar outcome...
> Hopefully, no body put those stuff (not in the plastic recycle bin that
> eventually went mixed with others) in some of bridge rebar coating or
> something like that... the half baked engineer plus politically
> correctness mentality is really scary.  (don't know what else of those
> friendly materials was into our life - both dvd and vhs are made in
> china... would think vhs would be safe -before friendly caught on
> fashion... but appear to be not the case...).  Try to pick up those small
> crystalline static dust is not fun... it is everywhere...
> on this cheery note, Have a nice weekend.
>                        jk
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2