Hi Mumtaz! I have a couple of questions and a couple of comments. Have you
run a solderability test per JSTD-002 Test Method S and if so what was the
result(s)? Has the customer been using that specific flux on these
components in the past successfully? A couple of things to consider - (1)
Pd is has a very slow diffusion rate (a couple orders of magnitude lower
than gold) and increasing the reflow profile by 5C can make a significant
difference; (2) NiPdAu surface finishes can have some flux sensitivity. I
have found some fluxes that are less robust to NiPdAu surface finishes
than others. Good Luck.
Dave Hillman
Rockwell Collins
[log in to unmask]
Mumtaz Bora <[log in to unmask]>
Sent by: TechNet <[log in to unmask]>
01/12/2010 04:56 PM
Please respond to
TechNet E-Mail Forum <[log in to unmask]>; Please respond to
Mumtaz Bora <[log in to unmask]>
To
[log in to unmask]
cc
Subject
[TN] NiPdGold Plating Soldering Issues
Hello Technetters,
We have some SC70 packages with NiPd gold plating that have wetting
issues .
Customer is using Kester R596L tinlead water soluble solder paste
conducting eutectic reflow at 227C peak and have wetting issues.(first
3 images in PowerPoint).
We have checked plating thickness with our supplier and it meets spec.
EDX did not show any contamination, oxides etc. JEDEC solderability test
passed.
X-section shows some areas of missing nickel or gaps in coverage of base
copper. I need the experts to look at the images and comment if this
could be the root cause of poor wetting and non-wetting.
I have forwarded the PowerPoint to Steven Gregory to post on his
website.
Your feedback will be much appreciated.
Thank-you
Mumtaz Bora
Senior Quality Engineer
Peregrine Semiconductor
9380 Carroll Park Drive
San Diego, CA 92121
858-795-0112-direct
858-731-9499 -fax
[log in to unmask]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|