In a message dated 5/16/06 12:48:44, [log in to unmask] writes:
> Any concerns yet amongst this group regarding planar microvoids and
> immersion silver?
> http://www.smta.org/files/oregon_chapter_presentation0905.pdf
>
Hi John,
Planar microvoids are indeed a reliability issue. Their connection to ImAg
has been shown to require what was termed "the perfect storm" of a rather
contrived combination of parameters. [ See Engelmaier, W., “Voids in Solder Joints—
Reliability,” Global SMT & Packaging, Vol. 6, No. 1 [EU Edition], December
2005/January 2006, pp. 44-45 & Cullen, Donald P., “Avoiding Microvoids,”
Assembly, September 2005.]
Werner
-------------------------------------------------------------------------------Leadfee Mail List provided as a service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Leadfree
To temporarily stop/(start) delivery of Leadree for vacation breaks send: SET Leadfree NOMAIL/(MAIL)
Search previous postings at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-------------------------------------------------------------------------------
|
|
|