Carrie,
Something that might be worth doing is a cross-section on the tinned area of
the wire to check on the extent of erosion of the copper wire strands.
SAC305 can be quite aggressive towards copper and if the strands are fine the area
reduction can be significant.
Keith Sweatman
Nihon Superior Co., Ltd